Sculpfun iCube Ultra IR 1.2W Laser Settings for Titanium
1 verified settings · manufacturer data · diode laser · Updated July 2026
| Operation | Mode | Speed | Power (%) | Passes | Air Assist | Notes |
|---|---|---|---|---|---|---|
| mark | — | 3 mm/s | 90% | 1 | — | Infrared laser for titanium marking. |
About Titanium Settings for the Sculpfun iCube Ultra IR 1.2W
The Sculpfun iCube Ultra IR 1.2W cuts Titanium cleanly at 2.5 mm/s with 90% power. Always test on a scrap piece first — every machine is slightly different, and variables like tube age, lens condition, and material batch can shift results.
For Titanium, the key variables to dial in are speed and power. If the laser isn't cutting through cleanly, slow down or add a pass before pushing power higher — excessive power causes charring and wider kerfs. Air assist is highly recommended for wood and organic materials to clear smoke and protect the lens.
Once you find settings that work, save them in Laser Lab to build your personal settings library. The AI predictor uses your calibrated results to suggest starting points for new materials automatically — so the more you log, the smarter it gets.
Frequently Asked Questions
What speed and power for Titanium on the Sculpfun iCube Ultra IR 1.2W?↓
For cutting Titanium on the Sculpfun iCube Ultra IR 1.2W, start at 2.5 mm/s speed and 90% power. These are manufacturer-verified starting points — always test on scrap first.
Do I need air assist for Titanium on the Sculpfun iCube Ultra IR 1.2W?↓
Air assist is strongly recommended when cutting Titanium. It clears smoke from the cut path, reduces charring, and helps protect your laser lens.
How many passes to cut through Titanium on the Sculpfun iCube Ultra IR 1.2W?↓
The manufacturer recommends 1 pass to cut through Titanium at 2.5 mm/s and 90% power. If the cut isn't clean, try reducing speed slightly before adding more passes.
Why isn't my Sculpfun iCube Ultra IR 1.2W cutting through Titanium?↓
Incomplete cuts are usually caused by incorrect power, speed, or focus distance. If edges are charred, try increasing speed or reducing power. If the laser isn't cutting through, reduce speed or increase power — or add an extra pass. Also verify your focal distance is correct for the material thickness and that your lens is clean.
More Settings for the Sculpfun iCube Ultra IR 1.2W
Titanium Settings for Other Machines
Save Your Own Sculpfun iCube Ultra IR 1.2W Settings
Track what works, get AI predictions for new materials, and share with the community. Laser Lab is free to start.
Save Your Sculpfun iCube Ultra IR 1.2W Settings
Track what works. Get AI-predicted starting points for any material.
Try Laser Lab Free →Download as PDF