2 verified settings · manufacturer data · fiber mopa laser · Updated July 2026
| Operation | Mode | Speed (mm/s) | Power (%) | Passes | Air Assist | Notes |
|---|---|---|---|---|---|---|
| score | Line | 2000 | 30% | 1 | — | Imported from WeCreat Lumos Ultra template id 0e1e4878-74d2-4b11-8fe4-c9f1995625b0. WeCreat source operation: engrave. WeCreat power key: 100w. WeCreat material type code: 2. Material slug hint: leather-synthetic. |
| engrave | Fill | 2000 | 30% | 1 | — | Imported from WeCreat Lumos Ultra template id 0e1e4878-74d2-4b11-8fe4-c9f1995625b0. WeCreat source operation: fillEngrave. WeCreat power key: 100w. WeCreat material type code: 2. WeCreat lineDesity: 300. Material slug hint: leather-synthetic. |
The WeCreat Lumos Ultra MOPA 100W cuts PU Leather Green/Black cleanly at 2000 mm/s with 30% power. Always test on a scrap piece first — every machine is slightly different, and variables like tube age, lens condition, and material batch can shift results.
For PU Leather Green/Black, the key variables to dial in are speed and power. If the laser isn't cutting through cleanly, slow down or add a pass before pushing power higher — excessive power causes charring and wider kerfs. Air assist is highly recommended for wood and organic materials to clear smoke and protect the lens.
Once you find settings that work, save them in Laser Lab to build your personal settings library. The AI predictor uses your calibrated results to suggest starting points for new materials automatically — so the more you log, the smarter it gets.
For cutting PU Leather Green/Black on the WeCreat Lumos Ultra MOPA 100W, start at 2000 mm/s speed and 30% power. These are manufacturer-verified starting points — always test on scrap first.
Air assist is strongly recommended when cutting PU Leather Green/Black. It clears smoke from the cut path, reduces charring, and helps protect your laser lens.
The manufacturer recommends 1 pass to cut through PU Leather Green/Black at 2000 mm/s and 30% power. If the cut isn't clean, try reducing speed slightly before adding more passes.
Incomplete cuts are usually caused by incorrect power, speed, or focus distance. If edges are charred, try increasing speed or reducing power. If the laser isn't cutting through, reduce speed or increase power — or add an extra pass. Also verify your focal distance is correct for the material thickness and that your lens is clean.
Track what works, get AI predictions for new materials, and share with the community. Laser Lab is free to start.